Difference between revisions of "Bethlehem Barracuda"
From Fritipedia
Jump to navigationJump to searchm (Barracuda moved to Bethlehem Barracuda: Moved to more specific title) |
m |
||
Line 1: | Line 1: | ||
− | + | Made by [[Bethlehem burners]] the Barracuda was designed specifically for [[flamework]] artists to be able to use both [[soft glass]] and [[borosilicate]]. It is a surface mix torch with an inner and outer flame. The centre flame has 6 jets and is useful for creating small details and the outer flame has 12 jets giving you a wider flame to heat your work. | |
Full flame gas consumption: 9 cu. ft./hr (239 l/hr); [[oxygen]]: 42 cu. ft./hr. (1192 l/hr) | Full flame gas consumption: 9 cu. ft./hr (239 l/hr); [[oxygen]]: 42 cu. ft./hr. (1192 l/hr) |
Latest revision as of 13:31, 13 November 2008
Made by Bethlehem burners the Barracuda was designed specifically for flamework artists to be able to use both soft glass and borosilicate. It is a surface mix torch with an inner and outer flame. The centre flame has 6 jets and is useful for creating small details and the outer flame has 12 jets giving you a wider flame to heat your work.
Full flame gas consumption: 9 cu. ft./hr (239 l/hr); oxygen: 42 cu. ft./hr. (1192 l/hr)
Will work upto 1" rod or 38mm heavy wall tubing