Vetrofond glass is manufactured in Italy. Many stockists of Vetrofond glass rods use their own colour descriptions and stock numbers. The last 4 digits used by any stockist for their stock numbers will refer to the Vetrofond factory stock number.
Vetrofond colours and stock numbers
Transparent
| Colour
|
Properties
|
Reactions
|
| 1004 clear
|
Colours appear lighter encased in clear
|
|
| 1005 crystal clear
|
good for encasing silver glass
|
|
| 1008 yellow
|
|
|
| 1012 light topaz
|
|
|
| 1014 topaz
|
|
Reacts with DH psyche to give purples and blues
|
| 1020 light grass green
|
|
|
| 1022 grass green
|
|
|
| 1024 dark grass green
|
|
|
| 1026 teal
|
|
|
| 1028 light emerald green
|
|
|
| 1030 emerald green
|
|
|
| 1034 light aquamarine
|
|
|
| 1036 aquamarine (aqua)
|
|
|
| 1038 pale aquamarine (light aqua)
|
|
|
| 1040 light purple
|
|
|
| 1042 purple
|
|
|
| 1044 dark purple
|
|
|
| 1048 grey
|
|
|
| 1052 light blue
|
|
|
| 1054 blue
|
|
|
| 1058 intense blue
|
|
|
| 1060 cobalt blue
|
|
|
| 1064 black
|
|
|
| 1068 pink
|
|
|
| 1069 electric yellow
|
|
|
| 1072 orange
|
|
|
| 1076 red
|
|
|
| 1080 pale lavender
|
|
|
| 1082 lavender blue (alexandrite)
|
|
|
| 1084 light brown
|
|
|
| 1086 medium brown
|
|
|
| 1088 dark brown
|
|
|
Opaque/pastels
| Colour
|
Properties
|
Reactions
|
| 1204 white
|
|
|
| 1206 anice white
|
|
|
| 1208 silk white
|
|
|
| 1212 pea green
|
|
|
| 1214 nile green
|
|
|
| 1216 grass green
|
|
|
| 1218 dark grass green
|
|
|
| 1220 periwinkle
|
|
|
| 1224 light sky blue
|
|
|
| 1228 dark sky blue
|
|
|
| 1232 turquoise
|
|
|
| 1236 dark turquoise
|
|
|
| 1240 light lapis blue
|
|
|
| 1242 lapis blue
|
|
|
| 1246 cobalt blue
|
|
|
| 1248 light grey
|
|
|
| 1250 medium grey
|
|
|
| 1255 flower pink
|
|
|
| 1262 dark ivory
|
|
|
| 1264 light ivory
|
|
|
| 1268 pearl grey
|
|
|
| 1272 violet
|
|
|
Specials
| Colour
|
Properties
|
Reactions
|
| 1408 medium yellow
|
|
|
| 1412 dark lemon
|
|
|
| 1420 coral
|
|
|
| 1424 carrot red
|
|
|
| 1428 light red
|
|
|
| 1432 medium red
|
|
|
| 1438 red purple
|
|
|
| 1444 light brown
|
|
|
| 448 dark brown
|
|
|
| 1456 gold pink
|
|
|
| 1460 yellow ocher (wasabi)
|
|
|
Odd lots
| Colour
|
Properties
|
Reactions
|
| 1801 cosmic storm
|
|
|
| 1802 apricot jam
|
|
|
| 1803 candy corn
|
|
|
| 1804 tomato soup
|
|
|
| 1805 orange dreamsicle
|
|
|
| 1806 smoke rings
|
|
|
| 1807 frog pond
|
|
|
| 1808 swamp moss
|
|
|
| 1809 jungle twilight
|
|
|
| 1810 lemongrass
|
|
|
| 1811 moon rock
|
|
|
| 1906 chardonnay
|
|
|
| 1909 transparent green odd
|
|
|
| 1910 transparent yellow odd
|
|
|
| 1911 silk white (opal white)
|
|
|
| 1912 olive green pastel
|
|
|
| 1917 Transparent amber (streaky amber)(antique amber)
|
|
|
| 1919 pale ivory
|
|
|
| 1922 transparent sage green
|
|
|
| 1925 transparent pale blue
|
|
|
| 1926 sea green (seafoam)
|
|
|
| 1927 ocean green
|
|
|
| 1931 river rock (brie)(avocado)
|
|
|
| 1932 fish pink
|
|
|
| 1933 pink no.3
|
|
|
| 1934 pink flower
|
|
|
| 1937 arancio perfecto
|
|
|
| 1938 pale aqua streaky
|
|
|
| 1939 intense tangerine
|
|
|
| 1943 orange sherbert (free range salmon pink)
|
|
|
| 1940 italian marble
|
|
|
| 1941 pineapple yellow
|
|
|
| 1942 watermelon (poppy)
|
|
|
| 1944 tangerine
|
|
|
| 1945 new white (custard)
|
|
|
| 1946 sunshine 1947 yellow ice (lemon ice)(belgian lace)
|
|
|
| 1948 banana cream
|
|
|
| 1949 lemon meringue
|
|
|
| 1951 transparent candy apple red
|
|
|
| 1952 violet odd (purplicious)
|
|
|
| 1954 cool white (odd cotton)
|
|
|
| 1955 seashell swirl
|
|
|
| 1957 orange punch
|
|
|
| 1958 pyjama blue
|
|
|
| 1960 light pink
|
|
|
| 1961 carrot red
|
|
|
| 1963 green tepenade
|
|
|
| 1964 pale avocado
|
|
|
| 1965 olive green
|
|
|
| 1966 dark olive green
|
|
|
| 1967 quartz grey
|
|
|
| 1968 slate blue
|
|
|
| 1969 pearl grey
|
|
|
| 1970 transparent streaky sapphire
|
|
|
| 1975 midnight blue
|
|
|
| 1976 key lime green
|
|
|
| 1977 parrot green
|
|
|
| 1978 transparent crystal green
|
|
|
| 1980 light streaky brown
|
|
|
| 1981 streaky brown
|
|
|
| 1982 dark streaky brown
|
|
|
| 1983 pale ocean blue
|
|
|
| 1984 pale moss agate
|
|
|
| 1985 moss agate
|
|
|
| 1986 lichen
|
|
|
| 1987 dark lichen
|
|
|
| 1988 pale crystal green
|
|
|
| 1989 transparent odd topaz
|
|
|
| 1990 honey crunch
|
|
|
| 1991 marbled avocado
|
|
|
| 1992 banana
|
|
|
| 1993 sweet lime (red jasper)
|
|
|
| 1994 strawberry sweet (dark red jasper)
|
|
|