Vetrofond glass is manufactured in Italy

Vetrofond colours and stock numbers
Transparent
1004 clear
1005 crystal clear
1008 yellow
1012 light topaz
1014 topaz
1020 light grass green
1022 grass green
1024 dark grass green
1026 teal
1028 light emerald green
1030 emerald green
1034 light aquamarine
1036 aquamarine (aqua)
1038 pale aquamrine (light aqua)
1040 light purple
1042 purple
1044 dark purple
1048 grey
1052 light blue
1054 blue
1058 intense blue
1060 cobalt blue
1064 black
1068 pink
1069 electric yelow
1072 orange
1076 red
1080 pale lavender
1082 lavender blue (alexandrite)
1084 light brown 
1086 medium brown
1088 dark brown
Opaque/pastels
1204 white
1206 anice white
1208 silk white
1212 pea green
1214 nile green
1216 grass green
1218 dark grass green
1220 periwinkle
1224 light sky blue
1228 dark sky blue
1232 turquoise
1236 dark turquoise
1240 light lapis blue
1242 lapis blue
1246 cobalt blue
1248 light grey
1250 medium grey
1255 flower pink
1262 dark ivory
1264 light ivory
1268 pearl grey
1272 violet
Retrieved from "https://www.frit-happens.co.uk/w/index.php?title=Vetrofond&oldid=331"

Navigation menu

Page actions

  • Page
  • Discussion
  • View source
  • History

Page actions

  • Page
  • Discussion
  • More
  • Tools
  • In other languages

Personal tools

  • Log in

Navigation

  • Main page
  • Recent changes
  • Random page
  • Help
  • Frit Happens! Forum

 

Tools

  • What links here
  • Related changes
  • Special pages
  • Printable version
  • Permanent link
  • Page information
Powered by MediaWiki
  • This page was last edited on 7 February 2011, at 08:48.
  • Privacy policy
  • About Fritipedia
  • Disclaimers