Revision as of 03:59, 14 November 2008 by Sparrow (talk | contribs) (New page: A marver is a tool for shaping beads. Usually made from graphite and in paddle form (well, a rectangular slim block on a wooden handle), it is really helpful to shape ends, tubes, bicones,...)
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)
Jump to navigationJump to search

A marver is a tool for shaping beads. Usually made from graphite and in paddle form (well, a rectangular slim block on a wooden handle), it is really helpful to shape ends, tubes, bicones, or to rub foil into a bead so it doesn't burn off as quickly when you put your bead back into the flame. Marvers do come in other shapes, including some fancy ones for special jobs.