Jump to content

ASK

From Fritipedia
Revision as of 12:01, 16 November 2008 by Jolene (talk | contribs)

ASK [glass]] used to be manufactured by Kugler amd is currently out of production but is still available in small quantities from a few stockists in a limited but bright colour palette. It is a brand of silver rich soft glass, compatible with Effetre, Vetrofond and other CoE 104 Glass rods.