Vetrofond glass is manufactured in Italy. Many stockists of Vetrofond glass rods use their own colour descriptions and stock numbers. The last 4 digits used by any stockist for their stock numbers will refer to the Vetrofond factory stock number.
Vetrofond colours and stock numbers
Transparent
| Stock Number
|
Colour
|
Properties
|
Reactions
|
| 1004
|
clear
|
colours appear lighter encased in clear
|
|
| 1005
|
crystal clear
|
good for encasing silver glass
|
|
| 1008
|
yellow
|
|
|
| 1012
|
light topaz
|
|
|
| 1014
|
topaz
|
|
reacts with silver glass - reacts with silver to produce organic effects
|
| 1020
|
light grass green
|
|
reacts with silver glass
|
| 1022
|
grass green
|
|
|
| 1024
|
dark grass green
|
|
|
| 1026
|
teal
|
|
|
| 1028
|
light emerald green
|
|
|
| 1030
|
emerald green
|
|
|
| 1034
|
light aquamarine
|
|
|
| 1036
|
aquamarine (aqua)
|
|
|
| 1038
|
pale aquamarine (light aqua)
|
|
|
| 1040
|
light purple
|
|
|
| 1042
|
purple
|
|
|
| 1044
|
dark purple
|
|
|
| 1048
|
grey
|
|
|
| 1052
|
light blue
|
|
|
| 1054
|
blue
|
|
|
| 1058
|
intense blue
|
|
|
| 1060
|
cobalt blue
|
|
|
| 1064
|
black
|
|
|
| 1068
|
pink
|
|
|
| 1069
|
electric yellow
|
striking
|
|
| 1072
|
orange
|
striking
|
|
| 1076
|
red
|
|
|
| 1080
|
pale lavender
|
|
|
| 1082
|
lavender blue (alexandrite)
|
|
|
| 1084
|
light brown
|
|
|
| 1086
|
medium brown
|
|
|
| 1088
|
dark brown
|
|
|
Opaque/pastels
| Stock Number
|
Colour
|
Properties
|
Reactions
|
| 1204
|
white
|
melts easily
|
|
| 1206
|
anice white
|
very shocky
|
reacts with [Effetre]] nero intenso
|
| 1208
|
silk white
|
|
|
| 1212
|
pea green
|
|
reduces in a propane rich flame
|
| 1214
|
nile green
|
|
|
| 1216
|
grass green
|
|
|
| 1218
|
dark grass green
|
|
|
| 1220
|
periwinkle
|
|
|
| 1224
|
light sky blue
|
|
reduces in a propane rich flame
|
| 1228
|
dark sky blue
|
|
reduces in a propane rich flame
|
| 1232
|
turquoise
|
|
reduces in a propane rich flame
|
| 1236
|
dark turquoise
|
|
reduces in a propane rich flame
|
| 1240
|
light lapis blue
|
|
|
| 1242
|
lapis blue
|
|
|
| 1246
|
cobalt blue
|
|
|
| 1248
|
light grey
|
|
|
| 1250
|
medium grey
|
|
|
| 1255
|
flower pink
|
|
|
| 1262
|
dark ivory
|
|
|
| 1264
|
light ivory
|
|
|
| 1268
|
pearl grey
|
|
|
| 1272
|
violet
|
|
|
Specials
| Stock Number
|
Colour
|
Properties
|
Reactions
|
| 1408
|
medium yellow
|
|
|
| 1412
|
dark lemon
|
|
|
| 1420
|
coral
|
|
|
| 1424
|
carrot red
|
|
|
| 1428
|
light red
|
|
|
| 1432
|
medium red
|
|
|
| 1438
|
red purple
|
|
|
| 1444
|
light brown
|
|
|
| 448
|
dark brown
|
|
|
| 1456
|
gold pink
|
|
|
| 1460
|
yellow ocher (wasabi)
|
|
|
Odd lots
| Stock Number
|
Colour
|
Properties
|
Reactions
|
| 1801
|
cosmic storm
|
|
reacts with silver glass - bleeds in to ivory glass
|
| 1802
|
apricot jam
|
|
|
| 1803
|
candy corn
|
|
|
| 1804
|
tomato soup
|
|
|
| 1805
|
orange dreamsicle
|
|
Reacts with [EDP]
|
| 1806
|
smoke rings
|
semi-transparent
|
|
| 1807
|
frog pond
|
|
|
| 1808
|
swamp moss
|
|
|
| 1809
|
jungle twilight
|
|
|
| 1810
|
lemongrass
|
semi-transparent
|
reacts with iris gold frit
|
| 1811
|
moon rock
|
striking
|
strikes from brick red to purplish coral
|
| 1906
|
chardonnay
|
|
|
| 1909
|
transparent green odd
|
|
|
| 1910
|
transparent yellow odd
|
|
|
| 1911
|
silk white (opal white)
|
|
|
| 1912
|
olive green pastel
|
|
|
| 1917
|
Transparent amber (streaky amber)
|
|
reacts with silver glass - reacts with ivory
|
| 1919
|
pale ivory
|
|
reacts with fine silver to produce organic effects
|
| 1922
|
transparent sage green
|
|
|
| 1925
|
transparent pale blue
|
|
|
| 1926
|
sea green (seafoam)
|
|
|
| 1927
|
ocean green
|
|
|
| 1931
|
river rock (brie)(avocado)
|
|
reacts with fine silver to produce organic effects
|
| 1932
|
fish pink
|
|
|
| 1933
|
pink no.3
|
|
|
| 1934
|
pink flower
|
|
|
| 1937
|
arancio perfecto
|
|
|
| 1938
|
pale aqua streaky
|
|
|
| 1939
|
intense tangerine
|
|
|
| 1943
|
orange sherbert
|
aka. free range salmon pink
|
reacts with silver glass
|
| 1940
|
italian marble
|
|
|
| 1941
|
pineapple yellow
|
|
|
| 1942
|
watermelon (poppy)
|
|
reacts with silver glass - reacts with ivory and fine silver
|
| 1944
|
tangerine
|
|
|
| 1945
|
new white (custard)
|
|
|
| 1946
|
sunshine 1947 yellow ice (lemon ice)(belgian lace)
|
|
|
| 1948
|
banana cream
|
|
|
| 1949
|
lemon meringue
|
|
reacts with Effetre copper green
|
| 1951
|
transparent candy apple red
|
|
|
| 1952
|
violet odd (purplicious)
|
|
reacts with fine silver and also ivory to produce organic effects
|
| 1954
|
cool white (odd cotton)
|
|
reacts with fine silver
|
| 1955
|
seashell swirl
|
|
reacts with fine silver and ivory
|
| 1957
|
orange punch
|
|
|
| 1958
|
pyjama blue
|
|
|
| 1960
|
light pink
|
|
|
| 1961
|
carrot red
|
this glass contains sparkles
|
|
| 1963
|
green tepenade
|
|
|
| 1964
|
pale avocado
|
|
|
| 1965
|
olive green
|
|
|
| 1966
|
dark olive green
|
|
|
| 1967
|
quartz grey
|
|
|
| 1968
|
slate blue
|
|
|
| 1969
|
pearl grey
|
|
|
| 1970
|
transparent streaky sapphire
|
|
|
| 1975
|
midnight blue
|
black rod with a blue core
|
|
| 1976
|
key lime green
|
|
|
| 1977
|
parrot green
|
|
|
| 1978
|
transparent crystal green
|
striking
|
strikes to neon yellow
|
| 1980
|
light streaky brown
|
|
|
| 1981
|
streaky brown
|
|
|
| 1982
|
dark streaky brown
|
|
|
| 1983
|
pale ocean blue
|
|
|
| 1984
|
pale moss agate
|
|
reacts with silver glass
|
| 1985
|
moss agate
|
|
|
| 1986
|
lichen
|
|
reacts with fine silver and ivory
|
| 1987
|
dark lichen
|
|
reacts with fine silver and ivory
|
| 1988
|
pale crystal green
|
|
|
| 1989
|
transparent odd topaz
|
|
reacts with silver glass
|
| 1990
|
honey crunch
|
|
reacts with fine silver and silver glass
|
| 1991
|
marbled avocado
|
|
reacts with fine silver and silver glass
|
| 1992
|
banana
|
|
|
| 1993
|
sweet lime (red jasper)
|
|
reacts with fine silver and silver glass
|
| 1994
|
strawberry sweet (dark red jasper)
|
|
reacts with fine silver and silver glass
|
| 1995
|
jupiter
|
|
reacts with fine silver and silver glass
|
| 1996
|
bloody mary
|
|
reacts with fine silver and silver glass
|
| 1997
|
painted desert
|
striking
|
|
| 1998
|
rhubarb
|
|
reacts with fine silver and ivory glass
|
| 1999
|
petrified wood
|
|
reacts with fine silver and ivory glass
|