Designed for the glass worker with limited high pressure fuel, this torch is intended to be highly efficient with its fuel whilst still being able to work with both soft glass and borosilicate. I has a 6 jet centre fire.

Full flame gas consumption: 5 cu. ft./hr (142 l/hr); oxygen: 12 cu. ft./hr. (341 l/hr)

Will work rod upto 16mm and tube upto 19mm

Further information

For more information see the The Bethlehem Betta Page