ASK [glass]] used to be manufactured by [[Kugler]] amd is currently out of production but is still available in small quantities from a few stockists in a limited but bright colour palette. It is a brand of silver rich [[soft glass]], compatible with [[Effetre]], [[Vetrofond]] and other [[CoE]] 104 Glass rods. | |||