New page: This is the point at which the glass begins to experience stress and if not annealed correctly these stresses will remain in the glass. The strain point varies for each glass depending on ...
 
No edit summary
Line 1: Line 1:
This is the point at which the glass begins to experience stress and if not annealed correctly these stresses will remain in the glass. The strain point varies for each glass depending on the manufacturer, elements contained within the glass and the [[coefficiency]] of the glass
This is the temperature at which the molecules in the glass stop flowing and moving.
Below this point if the bead has not been [[annealing|annealed]] correctly these stresses will remain in the glass. (unless the glass is then subsequently annealed).
 
The strain point varies for each glass depending on the manufacturer, elements contained within the glass and the [[coefficiency]] of the glass

Revision as of 14:35, 12 November 2008

This is the temperature at which the molecules in the glass stop flowing and moving. Below this point if the bead has not been annealed correctly these stresses will remain in the glass. (unless the glass is then subsequently annealed).

The strain point varies for each glass depending on the manufacturer, elements contained within the glass and the coefficiency of the glass