There are several bracelets systems available such as Troll, Pandora, Lovelinks, and Lovelinks petite to name a few. These are charm bracelets which people collect a range of beads on, including silver cored glass beads (aka [[silver cores]])
There are several bracelets systems available such as Troll, Pandora, Lovelinks, and Lovelinks petite to name a few. These are charm bracelets which people collect a range of beads on, including silver cored glass beads (aka [[silver core]]s)


The systems have different styles and sizes of chain and below is a guide to the sizes of the chains taken from posts on the Frit Happens forum.
The systems have different styles and sizes of chain and below is a guide to the sizes of the chains taken from posts on the Frit Happens forum.

Revision as of 16:29, 30 August 2009

There are several bracelets systems available such as Troll, Pandora, Lovelinks, and Lovelinks petite to name a few. These are charm bracelets which people collect a range of beads on, including silver cored glass beads (aka silver cores)

The systems have different styles and sizes of chain and below is a guide to the sizes of the chains taken from posts on the Frit Happens forum.

Troll 3.3mm across
Pandora 4.25mm across
Lovelinks 5mm across
Lovelinks Petite 3.5mm across