New page: Rechenback produce a limited range of colours in CoE 104. The opaque colours tend towards high colour saturation and so a little goes a long way. Dots made with the opaque Reichenback ... |
No edit summary |
||
| Line 1: | Line 1: | ||
[[ | [[Reichenback]] produce a limited range of colours in CoE 104. The opaque colours tend towards high colour saturation and so a little goes a long way. Dots made with the opaque Reichenback 104 glasses on a base bead of a very soft opaque colour (for example Effetre White) have a "bleed" effect rather than a crisp edge when melted down. | ||
Revision as of 23:23, 13 November 2008
Reichenback produce a limited range of colours in CoE 104. The opaque colours tend towards high colour saturation and so a little goes a long way. Dots made with the opaque Reichenback 104 glasses on a base bead of a very soft opaque colour (for example Effetre White) have a "bleed" effect rather than a crisp edge when melted down.