Line 22: Line 22:
|-
|-
| Effetre 106
| Effetre 106
|  
|
Clearer, less scummy version than Effetre 104.  Has both good and bad batches - the good batches are excellent.
 
| £3.00
| £3.00
|-
|-
Line 34: Line 36:
|-
|-
| Reichenbach
| Reichenbach
|  
|
Reichenbach clear comes in two varieties - soft and normal.  The normal works slightly stiff but has good clarity. 
 
| £7.00
| £7.00
|-
|-
| Lauscha
| Lauscha
|
 
|  
|Optically very clear, but prone to cracking over silver glass.
|-
|-
| Double Helix Zephyr
| Double Helix Zephyr

Latest revision as of 18:57, 19 November 2012

Clear glass does not equal clear glass - they are all different, and not even from manufacturer to manufacturer, but within different ranges. Most lampworkers at some point will want to use clear glass to encase a bead, which may lead to the bead cracking, if there are incompatibility issues, or a mucky surface, if the clear is not used correctly.

This page is looking to gather all the info we can on which clear does (and doesn't!) do what.

Clear glass comes in many different types and prices. The following table aims to summarise the various characteristics.


Glass Type Characteristics Price per 1/4 Kg (Tuffnells)
Effetre 104

Cheap and cheerful, probably the glass that came with your starter pack.

Prone to scumming then used with a Hot Head torch

£2.75
Effetre 106

Clearer, less scummy version than Effetre 104. Has both good and bad batches - the good batches are excellent.

£3.00
Vetrofond Apparently prone to scumming at higher temperatures but probably OK on Hot Head torch.
CIM Clear £2.75
Reichenbach

Reichenbach clear comes in two varieties - soft and normal. The normal works slightly stiff but has good clarity.

£7.00
Lauscha Optically very clear, but prone to cracking over silver glass.
Double Helix Zephyr This clear melts easily and smoothly, resists boiling and the resultant scumming, and should work well with silver. £17.00