Jump to content

Bethlehem Barracuda: Difference between revisions

From Fritipedia
Chameleon (talk | contribs)
New page: ==[http://www.bethlehemburners.com/bcuda.htm Bethlehem Barracuda]== The Bethlehem Barracuda was designed specifically for flamework artists to be able to use both soft glass and borosilic...
 
mNo edit summary
 
(2 intermediate revisions by the same user not shown)
Line 1: Line 1:
==[http://www.bethlehemburners.com/bcuda.htm Bethlehem Barracuda]==
Made by [[Bethlehem burners]] the Barracuda was designed specifically for [[flamework]] artists to be able to use both [[soft glass]] and [[borosilicate]]. It is a surface mix torch with an inner and outer flame. The centre flame has 6 jets and is useful for creating small details and the outer flame has 12 jets giving you a wider flame to heat your work.


The Bethlehem Barracuda was designed specifically for flamework artists to be able to use both soft glass and borosilicate. It is a surface mix torch with an inner and outer flame. The centre flame has 6 jets and is useful for creating small details and the outer flame has 12 jets giving you a wider flame to heat your work.
Full flame gas consumption: 9 cu. ft./hr (239 l/hr); [[oxygen]]: 42 cu. ft./hr. (1192 l/hr)


Full flame gas consumption: 9 cu. ft./hr (239 l/hr); oxygen: 42 cu. ft./hr. (1192 l/hr)
Will work upto 1" rod or 38mm heavy wall tubing


Will work upto 1" rod or 38mm heavy wall tubing
== Further information ==
For more information see the [http://www.bethlehemburners.com/bcuda.htm Bethlehem Barracuda Page]

Latest revision as of 18:31, 13 November 2008

Made by Bethlehem burners the Barracuda was designed specifically for flamework artists to be able to use both soft glass and borosilicate. It is a surface mix torch with an inner and outer flame. The centre flame has 6 jets and is useful for creating small details and the outer flame has 12 jets giving you a wider flame to heat your work.

Full flame gas consumption: 9 cu. ft./hr (239 l/hr); oxygen: 42 cu. ft./hr. (1192 l/hr)

Will work upto 1" rod or 38mm heavy wall tubing