Made by [[Bethlehem burners]] the Betta is designed for the [[glass worker]] with limited high pressure [[fuel]], this torch is intended to be highly efficient with its fuel whilst still being able to work with both [[soft glass]] and [[borosilicate]]. I has a 6 jet centre fire. | |||
Full flame gas consumption: 5 cu. ft./hr (142 l/hr); [[oxygen]]: 12 cu. ft./hr. (341 l/hr) | Full flame gas consumption: 5 cu. ft./hr (142 l/hr); [[oxygen]]: 12 cu. ft./hr. (341 l/hr) | ||
Latest revision as of 18:31, 13 November 2008
Made by Bethlehem burners the Betta is designed for the glass worker with limited high pressure fuel, this torch is intended to be highly efficient with its fuel whilst still being able to work with both soft glass and borosilicate. I has a 6 jet centre fire.
Full flame gas consumption: 5 cu. ft./hr (142 l/hr); oxygen: 12 cu. ft./hr. (341 l/hr)
Will work rod upto 16mm and tube upto 19mm
Further information