silverlemon

Thank you all, I had another play today...I was supposed to be working, oops.

I think the penny is starting to drop, only thing is I managed to get better colours from my rod of Terra where I melted the stubbies together and then struck them.....now I need to get those results in my beads.

I'll post again with today's results in a few days.
Bionic Sarah xxx    Sarah Downton On Facebook  My Etsy Shop

flowerjasper

they look fantastic!
such fab colours  ;)
sandy

Trudi


sparrow

Wow Sarah, they're absolutely fab! Love that top set!!!
Sabine x

www.littlecastledesigns.co.uk www.facebook.com/littlecastledesigns Ring Top Tutorial

Pam

Sarah they are fab. I just love the top set. I had given up on TN but you have inspired me.

saffie

wow Sarah they are beautiful i especially like this pink one in the top set!!!

silverlemon

Thanks guys, I think I'm starting to get to grips with this. I'm still not sure how to encase a bead with posh designs and not loose the colour, i.e. not like my encased donuts on the previous page, maybe I need to work cooler.  ;D
Anyway, I had a mega success yesterday with plain TNT2 over clear this time, will post pics when Dickie's sorted them.
Bionic Sarah xxx    Sarah Downton On Facebook  My Etsy Shop

TiaraHelen

Helen x

Even after all this time, the sun never says to the earth "you owe me".

♥♥Tan♥♥

Those colours are amazing, the best I have seen so far I think