Frit-Happens !
February 21, 2020, 07:14:56 PM *
Welcome, Guest. Please login or register.

Login with username, password and session length
your ad here
News:
Where are you?? Add yourself to the NEW FHF map here  | On flickr? Join our Frit Happens group: here

VISIT THE WIKI HERE
Get FH Status updates via twitter @FritHappens

 
   Home   Help Search Calendar Login Register  
Pages: [1]
  Print  
Author Topic: which wire?  (Read 1632 times)
0 Members and 1 Guest are viewing this topic.
flowerjasper
Forum Member
****
Posts: 470


Acorns!


WWW
« on: October 10, 2008, 05:08:33 PM »

i have just found a really useful conversion table , wire gauges,
need a bit of help, what i want to do is get some silver wire that i can use for bead wrapping and also so i can include beads in a chain maille bracelet,  ie the wire through the bead and curled twice at each end so it can be added,
would 1mm (20) be too thick?
sandy
Logged

mizgeorge
Administrator
*******
Posts: 786


Or should that be missus?


WWW
« Reply #1 on: October 10, 2008, 06:11:24 PM »

Not sure what conversion table you've found sweetie, but 1mm is 18ga. It's on the heavy side for wrapping with, but is great for simple loops. It might be that you're looking at SWG (which is not used a lot now) rather than AWG (also called B&S)?

If you're looking to only get one size, though, 20ga (0.8mm) is probably the best all-rounder. Make sure you get dead soft if you want to wrap. It's easier to harden than having to start annealing.

If you want some sample bits to compare, give me a shout and I'll pop them in the post for you.
Logged

flowerjasper
Forum Member
****
Posts: 470


Acorns!


WWW
« Reply #2 on: October 11, 2008, 03:18:17 PM »

thanks george,
when you say get it soft... what do i have to do??
s x
Logged

mizgeorge
Administrator
*******
Posts: 786


Or should that be missus?


WWW
« Reply #3 on: October 11, 2008, 03:21:55 PM »

LOL you just need to buy dead soft (sometimes called standard) wire. Half hard or full hard is too stiff to wrap with, but is great for earwires Wink Since I'm going to be posting to you anyway, I'll pop some samples in for you!
Logged

bluefairy
Forum Member
***
Posts: 141



WWW
« Reply #4 on: October 11, 2008, 03:58:31 PM »

 Grin Grin Grin  sorry, lowering the tone again, he he he, can't help but snigger a la teenager mode when reading all this smut advice  Cheesy
Logged

Helen xx

My Etsy     My Facebook     My Folksy
flowerjasper
Forum Member
****
Posts: 470


Acorns!


WWW
« Reply #5 on: October 12, 2008, 03:29:54 AM »

oooohhhh matron is this soft enough??? Grin