Author Topic: Liver of sulphur on sterling silver?  (Read 2490 times)
0 Members and 1 Guest are viewing this topic.
Amber
The quiet one
Forum Member
****
Posts: 341

Beads As Therapy


« on: October 10, 2008, 08:10:04 AM »

Can this be used to blacken sterling, or can it only be used on fine silver?  Huh
Logged

sparrow
I hold with those who favor fire.
Senior Forum Member
*
Posts: 869


I'm working on a dream...


WWW
« Reply #1 on: October 10, 2008, 08:14:39 AM »

No, sterling as well Smiley
Logged

Amber
The quiet one
Forum Member
****
Posts: 341

Beads As Therapy


« Reply #2 on: October 10, 2008, 12:10:43 PM »

Oh good, that's handy  Smiley

Thanks!
Logged

Dragonfire Glass
Forum Member
*****
Posts: 597



WWW
« Reply #3 on: October 10, 2008, 12:15:14 PM »

I've heard eggs work well too  Smiley
Logged

Shirley
Forum Member
******
Posts: 831


WWW
« Reply #4 on: October 10, 2008, 12:27:14 PM »

Some would say a little too well Wink
Logged

Val Cox Frit - Thai and Bali Silver 
Carol
the invisible woman......
Forum Member
****
Posts: 344


strawackie


« Reply #5 on: October 10, 2008, 12:27:24 PM »

I've got a bit of sterling languishing in horse urine at the moment......... Shocked (it's blackening nicely Wink )