in search of mini molds

Started by Evadark, February 07, 2008, 04:53:56 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

Evadark

I am trying to find some samll molds (that can fit into an SC-2 kiln) with muliple rectangluar shapes (4 - 6 to a mold perhaps?) I am trying to make some uniformly shaped rectangles for a project.

Searching the web Delphi Glass offers one (model 80642) but they are based in the uSA, can anyone recommend a UK supplier? All the ones I know of off hand seem to offer only larger molds.

Marie

♥♥Tan♥♥

check our martin tuffnells site he has them


Dizzy Di

Sorry just found this thread.
Tempsford glass, and creative glass at Gillingham both do small slumping molds.
Dia

Zeldazog

Warm Glass UK also do small ones, and I am sure I have seen a multiple one