Penglass
New Forum Member
*
Posts: 21


« on: September 23, 2015, 10:13:29 AM »

 Whenever i try and fuse with that textured dichroic it never comes out right but always with a bit of the edge showing or a distorted shap. Anyone know why?
Logged
Zeldazog
My name's Dawn, I'm an
Administrator
*******
Posts: 1048


I'm free, to do what I want...♪♪♪


« Reply #1 on: September 23, 2015, 01:37:40 PM »

A photo might help explain what you mean.

Also, are you using one or two layers, is it capped, what is your fusing program?

Logged

Penglass
New Forum Member
*
Posts: 21


« Reply #2 on: September 25, 2015, 05:41:37 AM »


How do I post  photo?Huh
I cap it and fully fuse at 804. I have tried both 3mm and 4mm glass as the warm glass site says dichroic is only 2mm.
Logged
Rascal
Forum Member
***
Posts: 188


« Reply #3 on: September 25, 2015, 07:41:28 AM »

Hi, I post photo's from Flickr. When you click on the photo you want in flickr, on the right hand side you get 4 icons, one of which is an arrow 'share photo'. If you click on the arrow, a box appears and you want the bbcode tab. Then you just copy and paste the link into your post on here. There is a choice of sizes, I normally do small or medium.

If you then do preview, you can check the photo appears before you click post.

Sorry can't help with posting from other sites or apps.

If this doesn't make sense, try doing a search on this forum (make sure you are on the main home page when using search) and I'm sure others have posted with answers that make more sense or using other apps/sites.
Logged
Margram
Temperature's rising
Forum Member
*****
Posts: 687


Glass in pocket


« Reply #4 on: September 25, 2015, 11:12:49 AM »

Are you remembering to cut the top layer of clear a bit bigger than the dichroic?
Logged

Zeldazog
My name's Dawn, I'm an
Administrator
*******
Posts: 1048


I'm free, to do what I want...♪♪♪


« Reply #5 on: September 25, 2015, 12:42:15 PM »


How do I post  photo?Huh


http://www.frit-happens.co.uk/forum/index.php?topic=23036.0
Logged

Penglass
New Forum Member
*
Posts: 21


« Reply #6 on: September 26, 2015, 04:24:39 AM »


I do cut the top layer bigger though I never seem to get it quite right, either too big or too small. I also tried Warm Glass's method of firing at 760 to get a more square cab but that's a disaster - they're just 'tacked' together. I'm very disheartned.....
Logged
Rascal
Forum Member
***
Posts: 188


« Reply #7 on: September 26, 2015, 07:35:41 AM »

Don't get disheartened, like anything it takes a lot of time and practise to get good at it. Not sure how long you have been doing fusing, do you live near someone you could have a lesson with?
Logged
flame n fuse
Forum Member
****
Posts: 464


WWW
« Reply #8 on: September 26, 2015, 12:14:32 PM »

have you tried to do the same with ordinary glass, not dichroic - and do you get the same problem?
Logged
Penglass
New Forum Member
*
Posts: 21


« Reply #9 on: September 27, 2015, 05:03:48 AM »

 I'm better with flat dichroic but any of the textured ones don't cover properly.Either they don't have enough topping or it spreads out past the dichro! It's a mystery.... I tried fusing at 780 last night and that was better though I didn't use any textured. x
Logged
flame n fuse
Forum Member
****
Posts: 464


WWW
« Reply #10 on: September 27, 2015, 12:19:37 PM »

this   http://harrachglass.blogspot.co.uk/2011/08/fusing-textured-dichroic-glass-with.html suggests putting clear frit into the dips - that might help the lack of topping problem.
Logged
Penglass
New Forum Member
*
Posts: 21


« Reply #11 on: September 27, 2015, 12:35:39 PM »

 OMG! I hadn't thought of that. That explains why it spreads out at 804. Will give it a go. Thank you Smiley
Logged
Moira HFG
Half Full Glass
Forum Member
****
Posts: 404


Ever the optimist


« Reply #12 on: September 27, 2015, 02:20:44 PM »

I hadn't seen the Harrach blog before - it's brilliant, thanks for the post!
Logged

Pages: [1]
  Print  
 
Jump to:  

Powered by MySQL Powered by PHP Powered by SMF 1.1.21 | SMF © 2015, Simple Machines Valid XHTML 1.0! Valid CSS!
Page created in 0.039 seconds with 19 queries.