Marcel

Today i made a borosilicate crystal with some inlcusions :)
and last week i have made a geode pendant :)





myrica

I love the geode. Having just started to make layered blobs for slicing, I can really appreciate the skills needed for your multiple layers.

Rascal

Amazing, they look really natural as if they've been made by nature.

Did you make the bear as well that is holding the crystal?

Marcel

Thank you  ;) and yes i made the bear too :)

Rascal

He is brilliant, and he looks so happy with his crystal.

Marcel

Thank you :) here is another borosilicate crystal :)
made yesterday :)


Pat from Canvey

I've run out of words so I'll just say WOW.

Marcel

Thank you :) this is what i made today! :)