Frit-Happens !
January 19, 2021, 08:04:23 AM *
Welcome, Guest. Please login or register.

Login with username, password and session length
your ad here
News:
Where are you?? Add yourself to the NEW FHF map here  | On flickr? Join our Frit Happens group: here

VISIT THE WIKI HERE
Get FH Status updates via twitter @FritHappens

 
   Home   Help Search Calendar Login Register  
Pages: [1]
  Print  
Author Topic: Spray A?  (Read 2625 times)
0 Members and 1 Guest are viewing this topic.
Sandera
Forum Member
***
Posts: 153



WWW
« on: February 10, 2013, 04:01:25 AM »

Me again! I've started working with float glass and have found that it loses its clarity after slumping. I don't dislike the finish (a bit cloudy but actually quite nice) however I keep hearing about devit spray that can be used to prevent the cloudiness. Has anyone heard of this or used it before? How does it work? I've seen a homemade recipe using borax, washing up liquid, distilled water http://www.glass-fusing-made-easy.com/devit-spray.html . Can it really be that simple? I know the best thing to do would be just to try the recipe but I would be interested in your thoughts.
Logged

Trudi
Forum Member
*******
Posts: 1674


This is me!


WWW
« Reply #1 on: February 10, 2013, 11:11:25 AM »

Is that the same as this (second item down)

http://www.tempsfordstainedglass.co.uk/acatalog/Devit_Spray_and_Liquid_Stringer_.html

I was advised to use this on fused glass that has been ground at the edges - it helps to remove the "tide" mark from the grinding! I clean the edges and then paint on with a fine brush and fire polish!
Logged

firedinglass
Forum Member
****
Posts: 267


WWW
« Reply #2 on: February 10, 2013, 11:25:11 AM »

I didn't find this much use, you're better off buying an ultra violet tester to find the tinned side. They don't cost much and always worked for me
Logged

Sandera
Forum Member
***
Posts: 153



WWW
« Reply #3 on: February 10, 2013, 01:47:18 PM »

Is that the same as this (second item down)

http://www.tempsfordstainedglass.co.uk/acatalog/Devit_Spray_and_Liquid_Stringer_.html

I was advised to use this on fused glass that has been ground at the edges - it helps to remove the "tide" mark from the grinding! I clean the edges and then paint on with a fine brush and fire polish!

Thanks Trudi. It's similar but it fires at a higher temperature I think. As I'm still experimenting I think I will start with homemade recipe and see what happens. Nothing ventured, nothing gained.
Logged

Sandera
Forum Member
***
Posts: 153



WWW
« Reply #4 on: February 10, 2013, 01:49:33 PM »

I didn't find this much use, you're better off buying an ultra violet tester to find the tinned side. They don't cost much and always worked for me

I read that it takes some doing to use it correctly and to be very, very careful with your eyes. It kinda put me off a bit tbh.

If you correctly identify the tin/air sides does this prevent clouding at the slumping stage?
Logged

Angie
Angie
Forum Member
**
Posts: 84



WWW
« Reply #5 on: February 10, 2013, 01:56:28 PM »

The Devit A solution from Tempsford glass has crushed glass in it and woks well, apparently the homemade one is a bit questionable as the glas is needed to coat the area....however the solution needs to be stirred with the paintbrush every time you apply it to suspend the glass or the results can be disappointing. Mind you, I havn't tried this with float glass.
« Last Edit: February 10, 2013, 02:04:53 PM by Angie » Logged

www.angiesnelling.com
In the future, all will be glass...
Sandera
Forum Member
***
Posts: 153



WWW
« Reply #6 on: February 10, 2013, 02:16:28 PM »

The Devit A solution from Tempsford glass has crushed glass in it and woks well, apparently the homemade one is a bit questionable as the glas is needed to coat the area....however the solution needs to be stirred with the paintbrush every time you apply it to suspend the glass or the results can be disappointing. Mind you, I havn't tried this with float glass.

Thanks Angie.

I think I'll try this out and let you know how I get on.
Logged

Glyn Burton
Forum Member
***
Posts: 149


WWW
« Reply #7 on: February 10, 2013, 03:29:55 PM »

The tin side of float glass is more prone to devit this can be minimised by not maintaining high temperatures for long periods and by crash cooling. I have used a hand held UV tester for years with no problems but I don't look straight into the lamp but it is very low powered. An old school way of testing is to put a small drop of water on to clean glass if the droplet becomes irregular then that is the tinned side. if it stays as a neat drop its untinned. Its not foolproof but with a bit of practice it works ok.
Logged
Sandera
Forum Member
***
Posts: 153



WWW
« Reply #8 on: February 10, 2013, 04:15:07 PM »

The tin side of float glass is more prone to devit this can be minimised by not maintaining high temperatures for long periods and by crash cooling. I have used a hand held UV tester for years with no problems but I don't look straight into the lamp but it is very low powered. An old school way of testing is to put a small drop of water on to clean glass if the droplet becomes irregular then that is the tinned side. if it stays as a neat drop its untinned. Its not foolproof but with a bit of practice it works ok.

I think I need to persevere with testing the sides using alternative methods. I've also heard that it's possible to tell by licking the glass!

The problem seems to be at the slumping stage. I used my usual slumping schedule which, in fact, didn't cause the piece to slump as much as I'd expected or wanted. So it looks as though I will have to either increase the temperature or hold for longer. Do you generally retain the clarity even after slumping?
Logged

firedinglass
Forum Member
****
Posts: 267


WWW
« Reply #9 on: February 11, 2013, 02:01:50 AM »

 Smiley
The tin side of float glass is more prone to devit this can be minimised by not maintaining high temperatures for long periods and by crash cooling. I have used a hand held UV tester for years with no problems but I don't look straight into the lamp but it is very low powered. An old school way of testing is to put a small drop of water on to clean glass if the droplet becomes irregular then that is the tinned side. if it stays as a neat drop its untinned. Its not foolproof but with a bit of practice it works ok.
Just what I was going to write, in all my years of fusing this is what I used and had no problems with devitrification  Smiley
Also maybe you need to look again at your slumping schedule and don't soak for too long
« Last Edit: February 11, 2013, 02:03:29 AM by firedinglass » Logged

Pages: [1]
  Print  
 
Jump to:  

Powered by MySQL Powered by PHP Powered by SMF 1.1.21 | SMF © 2015, Simple Machines Valid XHTML 1.0! Valid CSS!
Page created in 0.038 seconds with 19 queries.