Author Topic: Fusing a wire hook onto a single 3mm piece  (Read 1837 times)
0 Members and 1 Guest are viewing this topic.
Trudi
Forum Member
*******
Posts: 1674


This is me!


WWW
« on: February 08, 2013, 02:48:43 AM »

Hi

Is is possible to fuse a wire hook onto a single 3mm piece of glass - I tried it last night but the wire - nichrome came away.

Thanks x
Logged

Zeldazog
My name's Dawn, I'm an
Administrator
*******
Posts: 1048


I'm free, to do what I want...♪♪♪


« Reply #1 on: February 08, 2013, 02:56:00 AM »

Only by sandwiching it, Trudi - nothing really fuses to glass, other than glass (enamels are actually glass, decals are printed with ceramic or glass pigments, which contain glass...

You could put a small strip just where you want to add the wire, as opposed to over the whole piece (IYGWIM?)
Logged

Trudi
Forum Member
*******
Posts: 1674


This is me!


WWW
« Reply #2 on: February 08, 2013, 05:47:54 AM »