Thanks to everyone who came up with ideas for solving the torch flame problem. I carefully checked all the oxycon hoses for leaks and found none, but now oxycon is working fine and the torch flame is perfect and controllable. I wonder if a hose was partially blocked and moving them around has cleared something.
Anyway I have learnt lots by reading posts and playing around with torch, regulator and oxycon.......Now for some beads.
 