NO Gazzzzz!!

Started by Passionatelamper, December 05, 2011, 09:55:44 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

Passionatelamper

Hi can someone please help!! I was merrily making beads this evening, and made some nice lentils...when I thought the gas was going down in force. It is a new tank so its not that. I did have an additional torch a couple of weeks ago so a splitter has been put on the pipes leading to tank. I cannot see why the gas which has finally dissipated now...has died down...can someone please help? I am quiet nervous about this aspect in Glass making but have no one to help me here. Can someone tell me why this has happened? it just died off...thank you  :-\

etsy-header-dec12 by vonnie.t, on Flickr

Helen G

Have you altered the regulator maybe?

Passionatelamper

Hi Helen....Yesssss I did.....lol was quaking in my boots I can tell you....but got it to 3.5 Bar on large black screwy thing (Regulator)? on the top of the tank....I was bricking it.... lols... all done thank you hope you are ok? I am still shaking.....hehe! thank you :)  ;D

etsy-header-dec12 by vonnie.t, on Flickr