I have some millefiori left over from the microwave kiln firing fad - I think they're coe100 - will they be ok to add to beads do you think?

sarah t

no harm in trying and should be ok i would have thought ....use the 10% rule and i would not encase just in case

tinker

Ok Sarah, thanks - I'll try it, fingers crossed!

awrylemming

I made some coe 100 murrini (P & T) and decided to try them on effetre - it was problematic I have to say. Those that I didn't melt in simply popped off in the kiln.  Those I did melt in, only one didn't crack immediately, it waited a day.  I think it's because, unlike frit, it's a relatively large bit of glass in one spot, rather than dispersed equally (although I could be wrong and probably am!)  Always worth a try though.  ;D