julieHB

Well done, Rachel!  :) I advise to hang onto the beads for a while, though - sometimes cracks can develop quite a long time afterwards.
Julie xx

                           My Webbie - My Flickr

awrylemming

I've tried the cz thing, but after pinging about 10 of them across the floor (and never finding the little beggars again!) I gave up on them.  I may give the glue thing a try now  ;D

MangoBeads

Quote from: julieHB on September 04, 2011, 11:40:22 AM
Well done, Rachel!  :) I advise to hang onto the beads for a while, though - sometimes cracks can develop quite a long time afterwards.

Just posted the exact same advise on another thread :)

Rainbow

Can certainly vouch for that one, they can definately crack much later on  :'(