Stashmaster glass database updated

Started by Karen, August 20, 2011, 12:33:31 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

Karen

Karen




Stupid people shouldn't breed, but they DO!!

ARBeads

Mmm an update, have to consider that.

I have the original running on Runtime, fails to open on my antiquated version of Access. I've modded it quiet a bit to make the 3 digit codes the start of the DB scroll lists and referenced Tuffers names. Not sure if I can be A***d to phathom out how to transfer it all over to a new Stash!

This is a good Database with loads of info preloaded, at one point I even managed to get nearly all my glass labelled correctly but that has now gone to pot again due to me being lazy.
Ruth & Andy


www.etsy.com/shop/arjewellery for beads!

poledra1958

I am currently running version 1.2 but a new version should be ready soon,  I like it but I keep forgetting to remove glass as I use it  ;D

HH on Bulk,

tomcat

hmm - would like to have a look at it but when I click on the link for it - it just takes me back to the top of the thread ???
Mark - Blog - http://beadsbeerandphotos.blogspot.co.uk/
Life is not a game - its THE game, so play it like you mean it
A Long time ago in Egypt cats were worshipped as Gods, cats have not forgotten this !

Studio Girl


poledra1958

E-mail Debbie and she will e-mail you the new version.  I did and got a copy very quickly.

HH on Bulk,

Galloway Beads

If you click on the large wizard pic (not the small one) it seems to work.
HTH

Elaine xx

www.gallowaybeads.co.uk
My Etsy http://www.etsy.com/shop/Gallowaybeads

KatheL

Oooooh, this looks great, have just downloaded, now need to take some time to work out how to use it!
Thank you very, very much,
Kathe, Denmark
Kathe Lewis,
Denmark