Miriam

Still trying to find out all kinds of pink colors.





groetjes Miriam


Blog | Website | Colorcharts | Glasss

Marcel

Love the pink Miriam  8)
Here are a couple of Reticello's.









Stacy

Been thinking I've been neglecting our gallery so here are just some simple hearts:


Marcel

thanx everybody for the awesome comments  ;D
Here is another goblet i was practicing real hard last week
and finaly i could make what i had in mind for a long time here
it is  ;)




Marcel

Thanx and yep the top comes of:)

garishglobes

I've had fun this weekend - blown dragons designed to fit into (empty, so you can partly fill with lamp oil  ;) ) wine bottles:


Wine bottle dragon oil lamp - Blue by A flame with desire, on Flickr

and pendants inspired by (yes, honestly) my son's headmaster:


Mask - blue tears by A flame with desire, on Flickr


Mask - ashen by A flame with desire, on Flickr

sparrow

Ooooh, Emma, I'd missed the wine bottle dragon - how fab is he!!! And a beautiful goblet, Marcel!

From me, a very humble little bangle, that was actually a left-over from a larger piece of work that's not finished yet :)


Glass bangle by Sabine Little, on Flickr


Glass bangle by Sabine Little, on Flickr
Sabine x

www.littlecastledesigns.co.uk www.facebook.com/littlecastledesigns Ring Top Tutorial

Stacy


Stacy

Last one for a while now I promise!!  ;D



Steampunkglass

Excuse the hog, it's been ages since I've posted here  :-[ First some little paperweight marbles, they are about 30mm+ and use borostix - oh, how I love borostix! The photos don't really do them justice! Side and top photos;


And some more razors and some dip pens too  :)

Steampunkglass

Thank you everyone  :)
Quote from: garishglobes on April 20, 2011, 03:59:47 PM
I do love those pens, beautiful! Are they dip and write ones?
yes, I've seen 'Murano' ones but I figured the world needed some boro versions!  :D

I do like borostix for petals, they give a really nice 'texture' to the petals, and some of the light blues thin down and seem to have a luminous quality to them (or maybe it's just me!  ???) I've made lots more but don't have any finished ones here to photograph

Marcel

this morning i opened the kiln and here is my
Turtle  ;)




Steampunkglass

I'd be over the moon if I opened the kiln and found anything even half as good as that turtle! Wow!  :o

Marcel

thanx so much  ;) i just finished this piece
i am originaly a seed beader before i started flameworking
i just had to make this one

Steampunkglass

Been busy this week, lots of odd stuff! Firstly, a bit marble, made with indigo luster which makes such lovely metallic effects and ranges of colour. It's a a touch under 43mm and the biggest I've yet made. Two different angles on the marble;

These are fun, chopstick holders! I've made various leaf designs, and many of them rock slightly - I liked the idea that as leaves they are lightly trembling in the breeze, until the chop sticks are rested onto them to stop them moving. I also made some more cubic ones, but the organic shape ones I prefer (and are easier to make!)