What am I doing wrong?

Started by binty, March 09, 2011, 12:30:21 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

binty

I seem to be able to make a decentish bead, and am nearly always getting a nice pucker, but for some reason, quite a few of my beads (the only way I can describe it!) have a waist!

That is seem to be thicker on one side than the other, so say I make a bhb, then were to put a rivet thingy in, it would sit nicely on one side, but on the opposite side the glass wouldn't be touching the rivet.

I bet it's something really stupid I'm not doing!

hollergrafik

Sounds like the mandrel isn't straight when you are shaping up the bead, try putting an old mirror against the wall behind your torch. I did this and could see when the mandrel was tipping.

turnedlight

Or perhaps your bead release is too thick? ???
kathryn

hollergrafik

are you also reaming from both sides?

★★Terri★★

Do you mean that on one side of the bead it narrows slightly from both sides - bit like an hour glass shape?

If so I often get the same on bhbs (5mm mandrel).  I reckon it got some thing to do with the winding on - I use a hothead and do get a bit impatient.  I remedy it by shaping the bead as nicely as possible then add a little bit of glass at each side of the narrow bit - swipe one side forwards and the other backwards and melt them in.  Does that make sense?


turnedlight

kathryn

binty

Quote from: Terri on March 09, 2011, 06:32:05 PM
Do you mean that on one side of the bead it narrows slightly from both sides - bit like an hour glass shape?

If so I often get the same on bhbs (5mm mandrel).  I reckon it got some thing to do with the winding on - I use a hothead and do get a bit impatient.  I remedy it by shaping the bead as nicely as possible then add a little bit of glass at each side of the narrow bit - swipe one side forwards and the other backwards and melt them in.  Does that make sense?



That's exactly it!  I'll have another go tomorrow, and try and get some pics on.  Many thanks everyone x