Kalorlo

The little spacer of grasshopper I've made looks a good match to that shade on my monitor. Your monitor may vary  :D

helenfc

I have some green tea, my batch seems a lot more white than what you have Kaz (they are so pretty!) I agree the grasshopper is too green green. (if you know what i mean!)
Sabine that website looks awesome, her copper green is exactly what I'm looking for!! Mine is like the dirty copper green though. :(
And Krysia, I love your spacer organisation!! need to see if I have any pale emerald!
xx

Studio Girl

Reichenbach do one called mint green in 104 the same colour as you posted
Ionly have 1/2 rod other wise you would be very welcome to it
I am sure I got it from Martin if not it was Plowdens

Kalorlo

Is it definitely 104? Reichenbach's website has a mint green in 96 but not 104.

Studio Girl

Sure it was 104 I only had one rod and would love some more