House tidyish, dog walked, machines all doing there thing, kids parked in front of tv with games controllers in hand...I head off to the garage :)

I know what I want to do...a nice pretty blue covered in clear with pretty dots on it.

HAHAHAHA!!!! yeah right!!!  I now have some lovely blue beads....where did I go wrong? I was hoping for a coloured core not an entire coloured bead :(

Also where is the best place to buy etching fluid please :)

Bare with and all that...guaranteed more questions to follow....Such Fun  ;D ;D xx


turnedlight

Yes, all right Miranda ;D
I have both etching fluid and etching cream, both from Tuffnells. Everyone seems to swear by the fluid, I like it but I think the cream is more versatile.. Hope that helps a little?
kathryn

Redkite

I tried the same thing (and got the same result!!)

You either have to put a much thicker layer of clear, or use a slightly lighter shade for your dots, or etch the clear so the dots kind of stand out a bit more, but again, this works best with a thick encasing layer and will always be quite a subtle effect if the dots are a similar colour to the base.


Lush!

I'd say, start with a very small blue barrel, let it cool so that its no longer glowing at all, then add the clear. 

I like to start adding clear on the left edge and spiral wrap it round to the right hand side, then add a generous extra wrap of clear at each end - on top of the first layer of clear glass, not on the mandrel.

Keep your blue bead out of the flame the whole time you're encasing so that only the clear gets hot and the blue stays cooler.


www.lushlampwork.etsy.com

MadelineBunyan

yes, I'd second the extra thick clear on top of extra small blue, keeping blue nice and cool.

as for the dots on top, maybe try a white dot and then a dot of trans cobalt, to give it a background as it were, this might help them stand out a bit more. plus trans cobalt dots on white dots just look yummy anyway!

The Tartan Trout

Thank you :)

I thought it was probobly too much blue, not enough clear and the blue being too hot. They are actually quite pretty for a first attempt...will try again tomorrow :)

x