Colour Challenge 4 - BLUE - June 2007

Started by Les, May 29, 2007, 03:11:33 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

What's your choice for this months colour challenge ??? JUNE 07

pink
7 (25.9%)
blue
10 (37%)
ivory
7 (25.9%)
green
2 (7.4%)
yellow
1 (3.7%)

Total Members Voted: 18

Voting closed: June 01, 2007, 03:11:33 PM

Les

I'm sure that everyone knows that our Anna is on her jollies for a short while and so I have just posted a few choices for our next colour challenge...... Nice and summery I thought.....

Just holding the fort till Anna's back.... come and have your say :)

Les xx

Sarah

We're very quiet this month  :)

Here are mine. I'm very pleased with the colour combination - CIM bordello & french blue. But much less pleased with the post kiln cracks.   :'(

I've just checked Dora's thread & she recommends a much higher annealing temp for the french blue so that may be the problem.

Isabelle


LesleyMac

My entry for the blue bead challenge, hope its blue enough?

Lesley
Everyone is gifted, its just that some leave the wrapping on longer than others
(Richard Wilkins)


My Etsy http://www.etsy.com/shop.php?user_id=5469196

Phoenix*

Kim :)    &  www.phoenixbeads.co.uk