garishglobes

Better late than never!

Lets see some pictures  :D

Marcel


Miriam

I had the luck of watching Gail Crosman-Moore teach and she made me want to work with boro again. All the boro I had was gathering up dust for more then 4 years.  ;)

Trying to get the perfect pink I made these beads.







groetjes Miriam


Blog | Website | Colorcharts | Glasss

Marcel

thanx Everybody for the nice comments :D I love the colors Miriam  ;)
here are a bunch of hummingbirds there so much fun to make  :)



fionaess

I've been practising implosions......

pendant2 by Fiona1953, on Flickr


P1020849 by Fiona1953, on Flickr


pendant3 by Fiona1953, on Flickr


If it's got a hole, it's a bead !

garishglobes

Torch time at last!  :D

A quick marble -


Orchid marble by Flying Bead, on Flickr

and still working on these flat discs:


Flat blown disc by Flying Bead, on Flickr



garishglobes

Thank you folks  :)

A couple more - orchid knob:


Orchid knob by Flying Bead, on Flickr

and Mary (whose eyes are not quite as wierd in real life... ::)):


Mary by Flying Bead, on Flickr


Marcel

thank you everybody  ;) i love the orchid knob and marble  :)