would anyone like to share with me, how to use silver mesh so when encased you get that lovely effect with the glass pushing threw.

Rita

elburnzo


elburnzo

oh and i thought silver mesh left bubbles and copper mesh left the funny pushy through effect? did i make this up... its highly possible :P

Lyn G

Sherry Bellamy did a tutorial using copper mesh.....   http://www.etsy.com/listing/58302128/tutorial-how-to-use-the-chaos-copper

I must admit, I didn't manage to make it work....but then it was quite a while ago when I tried it.....perhaps I should have another go!   ::)


Jolene

It's brass mesh or wire or frit that gives you the bubbles.

Pat from Canvey

Rita, it's copper mesh that gives you the glass pushing through effect and it's much cheaper to start by practicing with the copper mesh than with silver. The silver is much less forgiving than the copper. Have a look at http://www.nanopod.tv/sherry_bellamy.html and scroll down to the bottom right for a chaos bead picture. Her tutorial is for sale at http://www.etsy.com/shop/SherryBellamy

Tills