Main Menu

Using silver foils

Started by ShinySnail, September 02, 2010, 09:27:10 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

ShinySnail

I have seen a few beads today on etsy that have silver patches on the surface and assumed they had just been rolled in silver leaf and parts burnt off...
I tried this evening but couldn't get the same effect - the silver patterns I got were similar but in comparison my beads looked messy and dirty! I tried to completley burn off some areas, but wasn't left with a clean bead in these spots.
Does anybody have any suggestions please?

The beads I saw had been etched and had bright shiny silver patches on - but i read somewhere that etching can dissolve silver leaf?
Perhaps i should be usig silver foil?

helbels

Do you have a link to any of the beads you've seen?  It might help us give you some tips on how the look you like was achieved.

Veebee

You can use a reduction flame (heavy propane, little oxy) in the areas you didn't burn off to bring out the shine on the silver. But more than that, you have to show us your beads!!!  ;D
Web: http://www.veebeads.net
The UK home of Val Cox frit!!
Fritt Flickr group: http://www.flickr.com/groups/1647822@N25/

ShinySnail


When I have a quiet 5 mins at work I normally look at pics of beads on here and etsy etc and email myself any images that give me ideas... I have looked and looked but I can't find where I pinched the picture from anywhere  :(

Feel bad about showing somebody elses beads without even awknowledging them, I have cropped the picture to show a part of the bead I'm talking about. Hopefully doing this wont offend anybody - apologies if it does, I'm not really sure on what is and isn't allowed re stuff like this!



It just looks really clean and bright, mine just looks like a murky mess but maybe I should have a go at etching it and see what happens...

I will post pics soon I promise, somebody has pinched my camera for a while and I have a months worth of first beads waiting to be unleashed upon the world!
 

ShinySnail

haaaaa look at how I spelt acknowledging  ;D

elburnzo

cant really see from the pic but is the silver maybe kept cool and encased in clear?