Started by sparrow, March 26, 2010, 05:35:35 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

sparrow

....can't you wait any longer and grab your beads out of the cooling kiln?  ;D ;D
Sabine x

www.littlecastledesigns.co.uk www.facebook.com/littlecastledesigns Ring Top Tutorial

Pandanimal

I normally put my kiln on over night so its well down to room temperature before its opened. but I think I would wait till its abut 35, 40c but that's just me being the cautious type.

sparrow

:) I normally give up as soon as there's a 4 in front and it's double digits...although I've been known to open the door at 52 to speed it up :)
Sabine x

www.littlecastledesigns.co.uk www.facebook.com/littlecastledesigns Ring Top Tutorial

turnedlight

#3
About 80-90, I pop them into something warm as well!
Mts only when I'm hanging about and not for big focals, usually I go out, come back and they are room temp - though it is hard to wait sometimes!
kathryn

Pat from Canvey


garishglobes

I anneal overnight so that I don't have to think about it!
I have been known to wake up at 4am and wonder what temp its at...but am usually too lazy to go and actually check

sparrow

Quote from: garishglobes on March 26, 2010, 06:29:07 PM
I anneal overnight so that I don't have to think about it!
I have been known to wake up at 4am and wonder what temp its at...but am usually too lazy to go and actually check
;D ;D ;D ;D ;D
Sabine x

www.littlecastledesigns.co.uk www.facebook.com/littlecastledesigns Ring Top Tutorial

Ilona

I used to take them out when the were under 40. Now my kilns outside and I also anneal over night so don't get to see them until the morning :)

Lush!

I anneal overnight too but if I've had a really late session the kiln is often still at around 150 ... so I may just crack the door to speed things along.  I take them out when they're below about 90  :-[


www.lushlampwork.etsy.com

Chameleon

we used to take blown glass out of the lehr anytime below 60, and if it was too slow getting down to temp we'd crack the lehr open at anything under 100 (altho only open about an inch) to cool it quicker so anything 70 or under and i will take beads out of the kiln

Amber


sublimekate

I've been know to whip em out at 100  ::) I figured my oven in the kitchen goes up to 240  ???

♥♥Tan♥♥

I don't know the temp but it hurts sometimes :-[

Margram

Quote from: Tan on March 26, 2010, 08:01:46 PM
I don't know the temp but it hurts sometimes :-[
;D

I usually wait til 50 now, just to be sure (but I used to be desperate and got them out at 100 (think the actual temperature of the beads was less than the read-out, to be honest).
Marg x  Etsy Flickr My blog

♥♥Tan♥♥

Did you have the burny thumb finger thing :D