best bead release?

Started by princess pink, February 24, 2010, 10:33:12 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

princess pink

Hey

what do you reckon is the best bead release? I'm due for some more and have been using fusion but find it cracks a fair bit.

any other reccommendations? i've tried dirty looie and it was shockingly bad!

amareargentum

I like Foster Fire - it has worked well whether air or flame dried

Carol

Quote from: princess pink on February 24, 2010, 10:33:12 PM

any other reccommendations? i've tried dirty looie and it was shockingly bad!

I'm one of the few who seems to like Dirty Looie - sorry I've no other recommendations Shahlaa, but if you stillhave some Dirty Looie left I'd love to do a trade with you :)
Carol

princess pink

Quote from: Carol (fed up with strawackie) on February 24, 2010, 10:51:13 PM
Quote from: princess pink on February 24, 2010, 10:33:12 PM

any other reccommendations? i've tried dirty looie and it was shockingly bad!

I'm one of the few who seems to like Dirty Looie - sorry I've no other recommendations Shahlaa, but if you stillhave some Dirty Looie left I'd love to do a trade with you :)

pm'ed you hun!

princess pink



princess pink

oo cheers kay, is the heavy duty one for something else?

I'm still not decided so other opinions greatly welcomed!

amareargentum

I got mine from Q, but the ebay supplier Kay suggests may be quicker and cheaper on postage.

MangoBeads

Having used all sorts of foster fire I now use Fusion plus for all my big beads and its good n strong - I have it on my webbie .

fionaess

Foster regular for soft and Best for boro...


If it's got a hole, it's a bead !

Helen G

I use fusion and since I stopped letting it get really hot (as in glowing mandrel) I don't have many problems. I even make my large focal hearts with it and so far, even though they take nearly 45 mins I haven't had an issue. Sometimes if I've used a press on the same bead more than a couple of times it will crumble off but other than that fine.
Now this is probably tempting fate but I have yet to have a bead that I can't remove from the mandrel either.

Jennie Lamb

Quote from: MangoBeads on February 25, 2010, 08:39:27 AM
Having used all sorts of foster fire I now use Fusion plus for all my big beads and its good n strong - I have it on my webbie .


I got some from Manda and it is the best I've used in my short time on the torch.  I used to get alot of cracking at the crucial moment and this one holds solid which is SO satisfying!!  Get it from Manda I say!!

squirsygirl

I use fusion, but have bought some 'bucket of mud' from Frantz.

BoM cleans a lot easier, but have yet to get it to flame dry, I have to dip and air dry in the house where it's warmer.

It's very thick, too.  I have to draw the mandrel out painfully slowly.

Kirsty

♥♥Tan♥♥

I'm a Foster fire girl, I love it and it can take all sorts

firedinglass

Foster fire, it does seem to dry out in the jar..but a bit of water and i'm OK again!


www.facebook.com/firedinglass
http://www.etsy.com/shop/firedinglass
Lisa