annealing temp for Bullseye beads?

Started by silverleaf, February 08, 2010, 09:40:24 AM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

silverleaf

Hi there

Could anyone tell me how best to anneal Bullseye 90coe beads? I can't see any info for rods on there website, but have seen elsewhere that they should be held at 516C - is that correct? And would a schedule similar to Effetre be ok in terms of the ramp speed? (I usually do 3.5 hrs to 520C, hold one hour, 2.5hrs to 420C then switch off).

Thanks for your help.

Helen

silverlemon

HI, I always anneal my Bullseye the same as my Effetre  :)
Bionic Sarah xxx    Sarah Downton On Facebook  My Etsy Shop

Trudi

Quote from: silverlemon on February 08, 2010, 09:51:31 AM
HI, I always anneal my Bullseye the same as my Effetre  :)

Me too - they all go in the same!

amareargentum

Oh Helen, have you been tempted by Bullseye! ;D

silverleaf

I just had to try those pinks! And so far so good - light fuschia is just to die for ;D

Thanks for the advice folks.