Bead Cube issues

Started by hot to trot, September 23, 2009, 05:17:36 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

hot to trot

Hi there, I am the proud owner of a fairly new bead cube. I finished batch annealing my stash and am now putting my beads straight in the kiln hot, having filled the kiln right up this afternoon I cannot get it to go from Programme 1 to Programme 2 so it would start ramping down immediately instead of waiting another 7 hours. Any one got any ideas about this.
Most grateful for any help.
Thanks, Jill

Zeldazog

Give Lee a ring, see if he's still there, I am sure he can talk you through it?

sarah t

its garaging now on programme 1 .... yes ?......you just preess and hold the up arrow for about 4 secs till bleeps..... this should forward it to 1 1/2 hour hold then ramp down (seg 2)

hope this helps  ;D

Lee - Kilncare

Quote from: sarah t on September 23, 2009, 06:24:42 PM
its garaging now on programme 1 .... yes ?......you just preess and hold the up arrow for about 4 secs till bleeps..... this should forward it to 1 1/2 hour hold then ramp down (seg 2)

hope this helps  ;D
Yup, bang on correct.

Hope you are all sorted now HtT ;)

TWITTER @kilncare
VISIT US ON FACEBOOK FOR THE LATEST ON US.
http://www.facebook.com/pages/Stoke-On-Trent-United-Kingdom/Kilncare-Ltd/238801689732

hot to trot

Hi there again, Thanks to those who answered, that sound great I will print it off and use it tomorrow. Love the kiln by the way, great for anyone who has little space or a beginner like me