Author Topic: My Silver Glass Tips (long!)  (Read 10991 times)
0 Members and 1 Guest are viewing this topic.
beadysam
BeadySamGlass.Com
Forum Member
*****
Posts: 635


I type before I think....


WWW
« Reply #15 on: April 03, 2007, 07:37:57 AM »

Its arrived!  I've got Van Gogh, Kandinsky and Rocio Silver Mist - I'm hoping to find time to play today Grin
Logged

glassworks
Guest
« Reply #16 on: April 03, 2007, 07:38:44 AM »

fabulous chap - let us know how you get on with it all!!! Cool
Logged
MyPrecious
Forum Member
****
Posts: 277



WWW
« Reply #17 on: April 03, 2007, 07:41:36 AM »

I think I'm going to have to buy some of this glass one day... Grin
Logged

Mary
Forum Member
*****
Posts: 656


WWW
« Reply #18 on: April 03, 2007, 09:28:35 AM »

Ooh, I've not tried Kandinsky!
Logged
Maikki
Forum Member
**
Posts: 56


« Reply #19 on: August 06, 2007, 09:10:57 AM »

I am still reading these older threads, just had to stop to write and thank! Earlier this summer I bought test rods of Double Helixes and have not made with them anything yet, just tried to get information of them. After reading Mary´s text I think I could try them - and now I understad WHY they are acting like they do. Thank you!
Logged

Maija-Leena
Mary
Forum Member
*****
Posts: 656


WWW
« Reply #20 on: August 06, 2007, 01:56:56 PM »

I'm glad it has helped you!
Logged
Pages: 1 [2]
  Print  
 
Jump to:  

Powered by MySQL Powered by PHP Powered by SMF 1.1.21 | SMF © 2015, Simple Machines Valid XHTML 1.0! Valid CSS!
Page created in 0.032 seconds with 19 queries.