Main Menu

Fibre blanket

Started by Jivesjools, January 22, 2009, 11:41:56 AM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

Jivesjools

How long do i need to leave the beads in the fibre blanket to cool?

Thanks

Rach
*Rachel*

www.jivesjools.co.uk



"Be kinder than nescesary as everyone one you meet is fighting some kind of battle"

Carol

Till you can pick them up without burning your fingers!  ;D
Carol

Kaz

Possibly up to an hour to ensure that they don't crack - some people may recommend longer but personally I like to have a peep well before that!!!
She's made of real glass. She got real real emotion. But my heart laughs I have that same sweet devotion!