Author Topic: Reichenbach "Show & Tell" Competition Prize Draw  (Read 21480 times)
0 Members and 1 Guest are viewing this topic.
Lush!
Julie
Forum Member
*******
Posts: 1145


Queen of Buttons :0)


WWW
« on: January 19, 2009, 10:22:05 AM »

Tuffnell Glass have very kindly offered a prize of a Glass Selection Pack (or two  Wink) to the winner/s of a prize draw to be drawn just before the Flame Off. 

How to Win:
All names will be put in to a raffle draw and a winner will be selected at random
Closing date is midnight on Easter Monday, 13th April 2009

The Rules:
All forum members are invited to enter – No minimum level of experience required
Your bead must be made with Reichenbach glass
You may use Reichenbach in combination with any other type of frit or glass rods
All glass used must be listed in your entry post
One picture per post please………
You may post as many times as you like,
Photographs of Reichenbach beads old and new are welcome.
Your name will be entered into the drawer for every bead you post…..
The more beads you post in the thread the more chances you have to win.

Good luck everyone!



(thanks to Jolene for letting me copy her rules from another thread!)
Logged

dinah46
Forum Member
****
Posts: 358



WWW
« Reply #1 on: January 19, 2009, 10:50:16 AM »

Would hate to disappoint Grin so here is antique clear with cim dirty martini and effetre black and white striped cane.

Logged

dinah46
Forum Member
****
Posts: 358



WWW
« Reply #2 on: January 19, 2009, 10:56:40 AM »

The lentil here is reichenbach magic and effetre black base with striped cane of effetre black and magic.  The small spacers are just magic and the patterned spacers are black base with striped cane swirls

Logged

Lush!
Julie
Forum Member
*******
Posts: 1145


Queen of Buttons :0)


WWW
« Reply #3 on: January 19, 2009, 12:09:48 PM »

The classic combo, Diane!  I'd forgotten about Magic!  I've got some of that!

I absolutely love that set Vicki, what a great shape  Smiley

Seeing as I'll be drawing the winner, I know I can't enter the competition but I can still Show and Tell  Wink

Reichenbach Mystic Beige with Reichenbach Porcelain and silvered ivory


Logged

Lush!
Julie
Forum Member
*******
Posts: 1145


Queen of Buttons :0)


WWW
« Reply #4 on: January 19, 2009, 12:12:44 PM »

Reichenbach Mystic Beige with a little Effetre straw yellow and silvered ivory


Logged

Lush!
Julie
Forum Member
*******
Posts: 1145


Queen of Buttons :0)


WWW
« Reply #5 on: January 19, 2009, 12:13:58 PM »

Reichenbach Porcelain with Effetre Violet



There's more, but I'll let somebody else get a word in  Cheesy


Logged

pixiewillow
Forum Member
***
Posts: 187



WWW
« Reply #6 on: January 19, 2009, 12:16:27 PM »


Opal rose




Logged

www.pixiewillow.etsy.com
www.pixiewillowdesigns.com
A mans idea of multi tasking is breathing & blinking at the same time.
julieHB
Global Moderator
*******
Posts: 886



WWW
« Reply #7 on: January 19, 2009, 01:32:04 PM »

Gorgeous beads already!!

This is antique green with Beadysam's Silver Dragon Candy frit:

Green lampwork bead earrings.
Logged

Julie xx

                            My Webbie - My Flickr
sparrow
I hold with those who favor fire.
Senior Forum Member
*
Posts: 869


I'm working on a dream...


WWW
« Reply #8 on: January 19, 2009, 02:02:56 PM »

Weeeell, she's Reichenbach (not that you won't have seen her elsewhere Wink)


..erm...Antique Clear. I'm struggling hard to find any that *aren't* Antique Clear, lol!

Logged

sublimekate
Forum Member
****
Posts: 288


I am Human


« Reply #9 on: January 19, 2009, 02:05:46 PM »

I haven't tried too many of the Reichenbach colours but I did do these last year and it's.....wait fot it..........................Antique Clear  Grin  with an antique clear and white twistie

Logged

Sarah
Mad Beady Woman and
Forum Member
****
Posts: 395


Flame Force Five


WWW
« Reply #10 on: January 19, 2009, 04:29:45 PM »

Great beads everyone - I'm especially loving those pinks Vickie  Smiley

These are antique crystal with aion - I'm quite fond of them  Smiley

<a href="http://www.flickr.com/photos/flameforcefive/3035693500/" >[/url]
Logged

Chameleon
I know the voices are not real, but they sure come up with some great ideas
Forum Member
****
Posts: 254



WWW
« Reply #11 on: January 20, 2009, 01:30:39 AM »

there are some gorgeous beads in here  Grin from me, yes you guessed, more antique clear !!


Logged

Pam
Forum Member
***
Posts: 224



« Reply #12 on: January 20, 2009, 02:02:32 AM »

Mystic beige.

Logged

Lush!
Julie
Forum Member
*******
Posts: 1145


Queen of Buttons :0)


WWW
« Reply #13 on: January 20, 2009, 12:34:03 PM »

Aren't the Mystics just soooo gorgeous!

Vicki, your nuggets look like Mystic Pink  Wink

I made some nuggets too, these are Reichenbach Silver Brown .... anybody else tried this glass?



I'd love to see what somebody good-with-silvered-glass can do with it!

Logged

Trudi
Forum Member
*******
Posts: 1674


This is me!


WWW
« Reply #14 on: January 22, 2009, 03:54:32 AM »



Made with Ocean over clear - it's hard to show on here how much this stuff sparkles!
Logged