I bought the pack, I can't seem to do anything right! A lot of them just seem to go black or grey ie burnt out I guess, I finally got a lovely colour in one, which was encased, and I noticed today that it's cracking in strange directions so I guess it doesn't like what I encased it with (vetrofond). Any tips?  :(
kathryn

Trudi

Got to admit that I have found it difficult to get reactions with too!!

dinah46

Me too - I get poop :(

Dizzy Di

I have been cooling it down in brass press, then reheating and then cutting out the oxygen until it goes black and flash through flame then into kiln.
I have found it does not like encasing :'( but put a bit of clear on top of a dot with white underneath has some nice effects too ;D
Hope this helps :-X

Dianne

Pat from Canvey

Is the Northstar pack boro or 104 glass. My Northstar small pack is all boro. Do they do a COE 104 pack too?

Trudi

Hi Pat

Yes Martin sells the COE 104

Dainne - thanks for the tips - will have to give it a go!

Mary

Which one is it? da Vinci 2 and van Gogh are strikers (like Terra and Luna), da Vinci 1, Monet, Silver Mist, Picasso and Chagall are reducing (like Kronos or Psyche).

A lot of silver colours can cause problems when encased. The Diamond Clear is the base for the other colours, so you know it will be compatible, and it's a nice sparkly clear.

Kaz

Does anyone know if there is a definitive guide to these colours there are some that I have no idea about - something like Garzoni which is a transparent green I think?
Kaz
She's made of real glass. She got real real emotion. But my heart laughs I have that same sweet devotion!

garishglobes

Well, I do know that Garzoni is that lovely pale green - its one of my favourites! It reduces and looks very pretty. Kandinsky also reduces and is a very dark rod. Isn't there a thread on Lampworketc somewhere that gives a list of all the silver colours and what they do?

turnedlight

Thanks guys, I will have a look - I haven't joined lampwork etc yet, but I guess it's time! I will try those colours you mentioned..