Which glass doesn't etch?

Started by sparrow, January 12, 2008, 08:46:28 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

*rowanberry*

Quote from: mizgeorge on January 13, 2008, 05:09:07 PM
Quote from: *rowanberry* on January 12, 2008, 08:55:21 PM
I had some vetrofond lavender (i think it was that one) which utterly refused to etch evenly just went grainy - very weird!

Were they the ones I got Claire? If so, they definitely don't look 'regular' etched, but I love them - kind of an ancient glass effect!

Yup they were.... blooming glass! I could have sworn for England that day as it wasnt a small set!

Sabine, you could encase anything you dont want to etch in CIM cirrus - its clear when used thinly. If you dont have any i can give you a couple of rods as I have a LOT of it as I got some free rods of it once.
Claire

sparrow

LOL, at the moment 'encase' and 'thinly' don't function in the same sentence for me, but I'll never say no to more glass  ;D When *are* we meeting on Friday, by the way?
Sabine x

www.littlecastledesigns.co.uk www.facebook.com/littlecastledesigns Ring Top Tutorial