Main Menu

104 clear glass

Started by short fuse, November 11, 2013, 08:12:29 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

short fuse

Hi, can anyone, point me in the direction of a good supplier that sells clear glass for fusing with 104 millefiori. I have found a couple of companies selling it but the sheets are small and quite pricey  :)

Pat from Canvey

A few years ago, I bought some 104 sheet from Martin at Tuffnells.

~tHePyRoPiXiE~

~ Chrystal ~
www.chrystalrosedesigncrafts.com

Pat from Canvey

Quote from: ~tHePyRoPiXiE~ on November 12, 2013, 10:09:12 AM

I know that Creative Glass do it...
http://www.creativeglassshop.co.uk/product/31829/effetre-glass-cristallo-50x50cm.html
Thanks for that Crystal, I'd forgotten them and they're only 40 miles from me accross the QE2 bridge.

~tHePyRoPiXiE~

They are the only place I know that do 104coe sheet in different colours aswell.
Millefiori chunks look cute on a coloured background, then capped with clear.
~ Chrystal ~
www.chrystalrosedesigncrafts.com

short fuse

Thanks all, I have just received a batch that I bought with some Millefiori and I've just popped them into the kiln  :)

Hopefully I get the desired effect tomorrow.

Will go and find Tuffnells now, many thanks

short fuse

#6
Just checked Tuffnells and it seems like they only sell rods and not flat sheets, will check out CGS now :)