What else will copper green react with?

Started by Kimster, June 23, 2013, 01:50:25 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

Kimster

I've made a couple of nice sets this weekend with a dark ivory base, & copper green & rubino oro. Just wondered if there's any other glass that Copper reacts nicely with? I've tried a couple of other opaque bases but the copper green looks really flat & boring  :-\ ...any ideas?

flame n fuse

I use a base of copper green, with stringers of eff acid yellow, coral and apricot yellow - they all give a thin back line. Also silver leaf can be interesting.

helbels


flame n fuse

interesting reactions with Reichenbach purple rose

Redhotsal

not a reaction tip, but I like to mix silvered ivory stringer and then etch the whole thing. It really looks gret etched.

Kimster

Thanks all, will have a little play tomorrow  :)

Alison G