Fenrir

Hi, a while back I bought a couple of packs of the mixed effetre stringers from tuffnels, in them I got two stringers that have a rough texture and are sort of redish pink but turn into a wide range of pinks depending on how long you heat them for. However I cannot seem to figure out what colour they are to order some more. Here is the stringer and a bead with three dots of it as petals



And here is the same stringer sitting on (from left to right) Dark red, medium red, light red, carrot red, and coral.



The colour in both of those pictures is off but the lentil is the closest to reality.

Kalorlo

Looks like coral to me (420). The exact shade varies a lot by batch so you can't always tell by putting one rod next to another. I think my coral stringers look darker than my rods too.

MyPrecious

Looks like coral to me too!
Kathy

My website

Curlybird

Wot they said - looks like coral to me as well, and mine is rough..

Anne
Anne

Fenrir

Thanks all, the rod's of coral that I have look sort of a peach colour rather than the redish pink of the stringers, but when I pulled a stringer from one once it cooled down it has changed colour to be more like the stringers I got in the pack. Thanks for the help :)