Mand

Hi all,

I have been admiring Pris' gorgeous Fire Lotus bead on FB and I remembered that I have a rod stashed away...  so, without wishing to waste some very expensive glass - how does it like to be treated?  Any tips on a base colour to use it over?  I was thinking dark ivory?  And then what do I do?

All advice gratefully received.

Thanks x

Shirl

I will be interested in this thread as well, as I only have half a rod and only dared use it once with some little dots.....I didnt do it right as it looked bobs.

Blue Box Studio

I found this on the TAG website http://www.taglass.com/PDFs/104WorkingTips2011.pdf does it help?  I have it pinned to my shedio wall, not that it's helping me.
Sue
Website ~ Etsy ~ Blog ~ Flickr

Lotti

Quote from: Blue Box Studio on September 23, 2011, 05:11:16 PM
I found this on the TAG website http://www.taglass.com/PDFs/104WorkingTips2011.pdf does it help?  I have it pinned to my shedio wall, not that it's helping me.

OH NO!  I wish you hadn't shared this Sue, just been reading it and now I want some and I really cannot afford any, what have you done!  :o :o ;D ;D ;D

Blue Box Studio

Sue
Website ~ Etsy ~ Blog ~ Flickr

Princess Peggy (Priscilla McGirr)

Those instructions are really useful Sue, and I've just printed them off.  I just got Fire Lotus and Dalai Lama from the Flame Off in April, and now I see the whole list of goodies I can't wait to try some of the others.  I put Fire Lotus over an ordinary cream base, and then heat, press, cool and strike, and then cool and strike some more, and then maybe reduce a little....the colours seem to get more intense in the kiln. Also I've used it in murrini.  Have got lovely blues and purples from Dalai Lama too, but havn't made much with it so far.
Pris
My Website http://www.dancingwithglass.co.uk  My Etsy http://www.etsy.com/shop/princesspeggy01
My Facebook page: https://www.facebook.com/DancingwithglassLampwork

Lotti

Um, mind you cheaper than some DH glass!  Lotti step away from the computer now  :o ;D  Love to see what you make with your Fire Lotus Mand and if you make one too Shirl. :)

Mand

#7
Ah, great thanks Sue and Pris. ;D


Have just read the destructions> " ...in general, Fire Lotus doesn't overstrike, it gets "poo" colors from not allowing the glass to cool enough between strikes."   Eeek!  This is what happened to my TAG Tibet a couple of years ago, I ended up with poo on a stick, very expensive poo on a stick! ::) :P

Blue Box Studio

My first efforts have been much the same.  Perhaps I should have listened to my mother's advice, 'if all else fails, read the instructions'!
Sue
Website ~ Etsy ~ Blog ~ Flickr

Fruddy

Righty ho!!!

I LOVE Fire Lotus - it is wonderful glass!    Here's a bead I made using it over Ivory....



To get the absolute best out of it, you need to chuck A LOT of heat at it..... you need the glass to go completely transparent and almost gloopy - nearly dripping off the mandrel!  Then cool it..... really really cool it, almost to the point where you are afraid that the bead may crack....

Then repeatedly strike it to get the gorgeous peacock pinks and purples....   

Lotti - I have tons of the stuff, if you would like a rod to play with, please PM me your address.


Shirl

I tried a few dots on ivery again today, got a bit of colour, but mainly poo......not a bit like Rachels :o

jobead

Me too, poo or a cracked bead.  :-[

Princess Peggy (Priscilla McGirr)

I get this:


fire  lotus by Princess Peggy1, on Flickr

And this is Dalai Lama:


dalai lama by Princess Peggy1, on Flickr

neither a very good shape, which is why they'll go in the fugley box.  Keep trying girls, it'll click eventually.
Pris
My Website http://www.dancingwithglass.co.uk  My Etsy http://www.etsy.com/shop/princesspeggy01
My Facebook page: https://www.facebook.com/DancingwithglassLampwork

Blue Box Studio

Wish my fuglies looked that pretty.  Mine really are fugly!
Sue
Website ~ Etsy ~ Blog ~ Flickr

Lotti

Quote from: Blue Box Studio on September 26, 2011, 11:28:35 PM
Wish my fuglies looked that pretty.  Mine really are fugly!

;D ;D ;D ;D  I agree!  I quite like those colours Pris :)