I think this is dark matter (am I right in thinking dark matter and multicolour dark are the same just named differently between Tuffers and Off Mandrel?)

It really likes presses and getting very cold before being wafted back in the heat.  It makes lovely ring topper flowers too, I'm wearing one now!


Dark Matter 001 by GaysieMay, on Flickr

Excuse the dust they've been on the window ledge for a week or two waiting to be etched - then a nice bracelet me thinks!
www.GaysieMay.etsy.com
www.facebook.com/gaysiemay

sparrow

Thy're yummy :) But no, Dark Matter is an Effetre colour, and Multi Dark is Reichenbach - my guess is that those are Multi Dark? :)
Sabine x

www.littlecastledesigns.co.uk www.facebook.com/littlecastledesigns Ring Top Tutorial

GaysieMay

I really must learn to label  ::)  Still it adds to life's little adventures - my glass is like a box of chocolate - you never know what you're gonna get!  ;D
www.GaysieMay.etsy.com
www.facebook.com/gaysiemay

Veebee

I'd agree, definitely multi dark, and definitely gorgeous!
Web: http://www.veebeads.net
The UK home of Val Cox frit!!
Fritt Flickr group: http://www.flickr.com/groups/1647822@N25/

SilverGems89

You've probably all seen it by now but just incase, Julie did some "secret" testing with for tuffnells you can find her results here  http://www.tuffnellglass.com/contents/en-uk/d101.html

Ciel

I also got some interesting colours if you really reduce it and I wrote a blog article regarding it's reactions: http://www.cielcreations.co.uk/blog/lampwork/dark-matter-effetre-glass/

LilLizaJane

Quote from: SilverGems89 on July 01, 2011, 06:35:53 PM
You've probably all seen it by now but just incase, Julie did some "secret" testing with for tuffnells you can find her results here  http://www.tuffnellglass.com/contents/en-uk/d101.html

Well, well, well - so that's who it was ;) ;) ;) I'd never have guessed! ;D
maintaining eccentricity in the midst of madness
www.LilLizaJane.etsy.com.  (aka Beth)

Redkite

I got a nice subtle reaction with ivory:



Dots and swirls are all dark matter, with SIS bands around the centre bead

awrylemming

Why on earth did I not think of using Dark Matter as decoration?  I always use it as a base.  Those are lovely beads.  :)