Margram

I had a similar experience this evening...started off with quite a small barrel of white, put two thick layers of violetty purple, encased with thick layer of clear and ended up with a frighteningly big blob with a mind of its own (it was about an inch and a quarter each way). Oh, and even though I was careful there were bubbles that I kept trying to burst and kept pushing back in. I'm telling you it must have taken me an hour to finally get it ready to pull! Got about three foot of pale lilac filigrano. Will show you if/when I put them on a bead ;D Thanks for the lovely clear tutorial, Trudi :) :-*
Marg x  Etsy Flickr My blog

Trudi

Keep at it, once you have it ready to pull you need to give it time so it's not too thin.